0574-62656998 kaiyuan99@163.com
Home > Heye repository > DFS

Heye repository

Thermally Conductive PA6

Thermally Conductive Material
Thermally Conductive Material is developed for the radiator of electronic products which require high thermally conductive and reduce the weight more than 50% compare with the same aluminum devices.

Features
>Good thermal conductive: 2-20W/mK
>Excellent thermal conductivity compared to normal
engineering plastics
>Light than normal Aluminum housing 50% in weight
>Excellent mouldability in injection moulding
>Much higher production yield than normal Aluminum Die Casting
>Excellent flexibility in designing final pruducts such as housings.
>Flame resistance, UL94 V-0

Application
Used in applications such as Heat Sinking Housing at LED-lit BLU in LCD/LED TV and LED-lit lamps Also it can replace the normal Aluminum heat sink.

3-3.jpg


Typical Properties

Item                             Test method              Unit          KY661  KY662   KY663
Physical Properties
Color Visual                                                                     Black  White  White
Specific Gravity           ASTM D792             -                  1.48   1.7       1.6
Shrinkage                                                      %                          0.05 - 0.1
Continuous Use Temp °C                                                        -20 to 150
Mechanical Properties
Tensile Strength,         ASTM D638           Kgf/cm2         115     110    130
Flexural Strength        ASTM D790            Kgf/cm2         168     160    200
Flexural Modulus        ASTM D790            Kgf/cm2        16300 12300 15000
Impact Strength, notched ASTM D256     Kgf.cm/cm       45        55    70
Electrical Properties
Volume Resistivity     ASTM D257           Ohm-meter                4000
Thermal Properties
Heat Deflection Temperature ASTM D648   °C                  205   205   205
Thermal Conductivity in plane Research center W/m-K     3       1.2        1.0
Flame retardance Min. thick. 1.0mm Class                        V-0 V-0 V-0


Processing Date:
Injection Nominal Value Unit
Drying Temperatur e 100 °C
Drying Time 3-4.0 hr
Rear Temperature 260-290 °C
Middle Temperature 270-300 °C
Front Temperature 270-300°C
Nozzle Temperature 270 -300°C
Mold Temperature 80.0 to 100 °C
Screw Speed 30 to 150 rpm